Welcome to GPMR GLOBAL. Leading Supplier of Natural & Synthetic Rubber
Home Synthetic Rubber Reprocess
REPRO S-SBR synthetic rubber offers low rolling resistance, and wet grip. It also provides cost advantages to our customers. It provides a high level of color sensitivity in the production of colored rubber compound. Both oil extended and non-oil grades are available. Our oil extended grades of S-SBR are suitable for the use of products subject to PAH (Polycyclic Aromatic Hydrocarbon) tests due to their TDAE type oil content.
COLOR
SSBR Non-Oil: White, white to cream, white to grey (Both colors are suitable for colored compounds)
SSBR Oil: Brown and soft brown (Soft brown is suitable for colored compounds)
APPLICATIONS
Solid Tyre - Rubber Retread - Shoe Sole - Rubber Conveyor Belt - Rubber Compound
Specification SSBR Non Oil
| Properties | Unit | Value | Test Method | |
|---|---|---|---|---|
| Mooney Viscosity* | MU | 50 - 70 | ASTM D 1646 | ![]() |
| Bound Styrene | % wt. | 15 - 22 | SM** | |
| Vinyl Content | % wt. | 30 - 60 | SM** | |
| Moisture Content | % wt. | 1.5 max. | Internal Method | |
| Density | (g/cm3) | 0.94 | Internal Method | |
| Stabilizer | Non-Staining | SM** |
*ML 1+4 (100°C) unmassed sample | **Supplier Method
Specification SSBR Oil
| Properties | Unit | Value | Test Method | |
|---|---|---|---|---|
| Mooney Viscosity* | MU | 50 - 80 | ASTM D 1646 | ![]() |
| Bound Styrene | % wt. | 20 - 40 | SM** | |
| Vinyl Content | % wt. | 30 - 60 | SM** | |
| Oil Content (TDAE) | % wt. | 30 - 37.5 | Internal Method | |
| Moisture Content | % wt. | 1.5 max. | Internal Method | |
| Density | (g/cm3) | 0.94 | Internal Method | |
| Stabilizer | Non-Staining | SM** |
*ML 1+4 (100°C) unmassed sample | **Supplier Method
BR Repro synthetic rubber offers good abrasion resistance and high elasticity with an excellent processing behaviour to our customers. It also provides cost advantages to our customers. It provides a high level of colour sensitivity in the production of coloured rubber compound. Both high cis and low cis grades are available.
High Cis BR is a reprocessed polybutadiene elastomer with neodymium catalyst. It is reprocessed It provides good abrasion resistance and high elasticity with an excellent processing behaviour.
COLOR
White to amber, Grey (Both colors are suitable for colored compounds)
APPLICATIONS
Solid Tyre - Rubber Retread - Shoe Sole - Rubber Conveyor Belt - Rubber Compound
| Properties | Unit | Value | Test Method | |
|---|---|---|---|---|
| Mooney Viscosity* | MU | 43 - 63 | ASTM D 1646 | ![]() |
| Cis Content | % wt. | 95 - 97 min. | SM** | |
| Moisture Content | % wt. | 1.5 max. | Internal Method | |
| Density | (g/cm3) | 0.91 | Internal Method | |
| Stabilizer | Non-Staining | SM** |
*ML 1+4 (100°C) unmassed sample | **Supplier Method